Glassy polyamide 6 was obtained by quenching the melt in liquid toluene at 210°K. On the DSC thermogram of such a polyamide a small endothermic peak of glass transition at 310°K, and an exothermic peak at 325°K of cold crystallization are observed (both temperatures were calculated by extrapolation to zero heating rate). The kinetics of cold crystallization was investigated in the range 321‐339°K by DSC technique using three different methods of measurement: 1) standard isothermal, 2) isothermal by Miller, and 3) nonisothermal by Ozawa. The data obtained from 1 and 2 were analyzed by the simple Avrami equation, and from 3 by a modified equation. It was confirmed that the exponent n is not constant; in the range up to 328°K it has an average value of 2.2, and then varies with the rise in crystallization temperature. Unfortunately, the mechanism of the variation of n is not known and this prevents the calculation of the crystallization rate from the nonisothermal dynamic data. Thus, an assumption was made that crystallization follows first‐order kinetics: K and t 0.5 for different temperatures were calculated; the Arrhenius function was plotted; and from it the activation energy of 69.7 kcal/mole was estimated.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Wojciech Kozłowski (1972) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: