This is the authors' abstract. We don't add key points for this paper.
Sb 2 O 5 -doped tin-oxide (SnO 2 ) thin films were prepared on glass substrates by using pulsed laser deposition (PLD). The electrical and the optical properties of these films were investigated by varying the doping amount, oxygen partial pressure, substrate temperature, and film thickness. The electrical properties were studied through the resistivity, the Hall mobility and the number of carriers measured as functions of the conditions. The best value of the resistivity of the films was 7.8 × 10 −4 Ω·cm and the average transmission in the visible region was 84% at a substrate temperature of 500 °C and doping amount of 6 wt.%. The figure of merit was computed from the spectral transmittance and the film-thickness-dependent resistivity. The lowest resistivity (7.8 × 10 −4 Ω·cm) was observed for the annealed film deposited with a doping of 6 wt.%.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Seo et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: