A method to control the two-dimensional electron gas (2DEG) density in AlGaN/GaN heterostructures through post-epitaxial device processing is investigated. This control was achieved by dielectric film deposition and subsequent annealing on an ultra-thin 5-nm Al0.22Ga0.78N barrier layer. The 2DEG density, estimated from sheet resistance assuming constant mobility, was found to be tunable from 8.3 × 107 cm−2 before dielectric film deposition to 4.5 × 1012 cm−2 after SiO2 film deposition and annealing. Hard x-ray photoelectron spectroscopy analysis confirmed a maximum shift of 0.8 eV in the surface pinning level, attributed to the dielectric film deposition and annealing. Numerical calculations indicate that for an AlGaN barrier layer thickness of approximately 5 nm, a surface pinning energy change of ∼0.8 eV can induce a 2DEG density variation of 6–8 orders of magnitude, supporting the validity of the experimental results.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Nanjo et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: