This is the authors' abstract. We don't add key points for this paper.
The small-signal ac permittivities (ε) of single crystal samples of KDP, BaTiO3, and TlCl, and of a ceramic sample of PZT 65/35 have been measured as a function of temperature between 0.015 and 10 K. For KDP and PZT 65/35, ε increases essentially linearly with temperature in this range, with d In ε/dT = 0.95 ± 0.15 × 10-3 K-1 and 1.81 ± 0.02 × 10-3 K-1, respectively. For BaTiO3 linear behavior is observed only between 1.5 and 4.5 K, with d In ε/dT = 9.4 × 10-4 K-1. PZT 65/35 exhibits positive deviation from this apparent linear behavior between 0.1 and 1.5 K, while BaTiO3 shows a negative deviation in this range. Both PZT 65/35 and BaTiO3 have a minimum in ε below 0.1 K and an associated change in the dielectric loss factor that depends on the frequency and amplitude of the ac signal. No temperature dependence of ε was observed below 3 K for TlCl. Potential applications of these materials at low temperatures are discussed.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Holste et al. (1976) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: