Answers are grounded in this paper and cite their sources.
We report the effect of N2O post-fabrication annealing (PFA) on the electrical stability of dual gate, active split amorphous indium gallium zinc oxide (a-IGZO) thin-film transistor (TFT). Optimized N2O PFA at 360 °C for 3 h results in threshold voltage (VTH) close to zero and an increase in the on-current almost 2 times than as-fabricated TFT. N2O annealed TFT exhibited robust VTHstability under positive bias temperature stress at 60 °C and negative bias illumination stress, exhibiting ΔVTHof 0.1 V ,and0.1 V, respectively, whereas as-fabricated TFT showed large ΔVTHof ~ 10 V and -3 V. The X-ray photoelectron spectroscopy depth profile reveals the origin of such improvement as the increasing metal-oxide bonds and the reduction in oxygen vacancy/ OH related defects.
No takes yet. Share an insight, caveat, or question.
Rabbi et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: