Answers are grounded in this paper and cite their sources.
A promising strategy for enhancing the mechanical properties of sputtered transition metal diboride (TMB 2 ) thin films, including hardness and fracture toughness, is the formation of ternary diborides. Theoretical calculations indicate that incorporating Mo on the metallic sublattice of TiB₂ enhances the overall mechanical properties; however, no experimental data are available. Accordingly, two series (DCMS & HiPIMS) of Ti 1-x Mo x B 2±z coatings with varying Mo contents (x = 0 to 12 for DCMS and x = 0 to 9 for HiPIMS) were deposited using TiB 2 /MoB composite targets containing different MoB contents to investigate their structural and mechanical properties, focusing on fracture characteristics. HiPIMS growth processes have been proven to significantly enhance hardness, fracture toughness, and fracture strength compared to DCMS. Specifically, a hardness increase from 38.8 ± 1.7 GPa to 43.7 ± 1.2 GPa (nanoindentation) with a simultaneous fracture toughness increase of 0.4 MPa√m (~17 %; using microcantilever bending tests) and an increase in fracture strength, R p0.2 of approximately 2 GPa (micropillar compression) was observed for HiPIMS deposited coatings. Compared, our DCMS coatings showed a steady decrease in mechanical properties from H = 38.3 ± 1.5 GPa, K IC = 2.6 ± 0.15 MPa√m and R p0.2 = 13.7 ± 1 GPa to H = 27.2 ± 0.4 GPa, K IC = 1.7 ± 0.06 MPa√m and R p0.2 = 9.3 ± 0.3 GPa with increasing Mo content. Our research emphasizes the significance of energetics during film growth, particularly for new ternary diboride systems. • Successful deposition of Ti 1-x Mo x B 2±z thin films by using DCMS and HiPIMS • Influences of Mo and deposition technique on Ti 1-x Mo x B 2±z thin films were shown. • Enhanced micromechanical properties for HiPIMS deposited coatings
No takes yet. Share an insight, caveat, or question.
Hirle et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: