A PbTiO 3 ferroelectric film 813 Å thick was grown on a CeO 2 /Si(100) substrate by the digital chemical vapor deposition method. As the buffer layer between the perovskite PbTiO 3 film and Si substrate, a CeO 2 intermediate layer was grown on the Si(100) substrate using an ultrahigh vacuum (UHV) system. The density of surface states at the CeO 2 /Si(100) interface was estimated from the capacitance-vs-voltage ( C - V ) characteristics of Al/CeO 2 /Si(100) samples to be 8×10 11 /cm 2 eV, and CeO 2 films on Si(100) are therefore expected to be suitable as gate oxides for metal/ferroelectric/semiconductor-field-effect transistors (FETs). Experimental results derived from the C - V characteristics of metal/ferroelectric/insulator/semiconductor (MFIS)-structured samples show that the MFIS structure has ferroelectric switching properties, as demonstrated by the roughly 2.4 V threshold hysteresis in its C - V characteristics (“memory window”). Furthermore, the retention time of the MFIS sample was estimated to be 100,000 s by measuring the time dependence of capacitance at the voltage at the centuer of the memory window. Interfacial lines of the MFIS structure were clear in a transmission electron microscope image, and an amorphous CeO x layer and an amorphous SiO 2 layer were seen between the Si substrate and PbTiO 3 film. Secondary ion mass spectroscopy revealed that there was little diffusion of Si atoms into the PbTiO 3 layer on the CeO 2 /Si substrate.
No takes yet. Share an insight, caveat, or question.
Hirai et al. (1995) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: