Deformation behavior of electrodeposited plates of pure iron was studied. The plate consisting of fine cdamnar grains with (III) fiber texture was found to show Rankford (γ) value as large as 7.6 at 293K. When test temperature was lowered to 77k, the r-value was decreased. The r-value was also decreased when specimens were annealed to enlarge grain size. From observations of surface believes and substructures of deformed specimens, it is speculated that such an extromoly high r-value is mainly caused by grain boundary sliding.