Answers are grounded in this paper and cite their sources.
CeO 2 powders have been prepared by aging a cerium(III) nitrate solution in the presence of hexamethylenetetramine. Oxidation of Ce 3+ occurs in the precipitate and the wet precipitate is identified as crystallized CeO 2 before any heat treatment. The cold‐pressed powders can be sintered to full density at temperatures as low as 1250°C in just 6 min. Moreover, the sinterability of the powders is insensitive to the calcination temperatures, particle size, or green density. The powders calcined at 850°C with a crystallite size of 600 Å have a sinterability as good as the powders calcined at 450°C with a crystallite size of 145 Å. The mechanisms for direct CeO 2 precipitation and its relation to the excellent sinterability are discussed.
No takes yet. Share an insight, caveat, or question.
Chen et al. (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: