Answers are grounded in this paper and cite their sources.
Measurements of the thickness dependence of the electrical resistance of two very thin Cr films deposited at substrate temperatures of 385 and 360 °C and pressures of 4×10−7 and 10−6 Torr are reported. Preliminary measurements of the thickness dependence of the Néel temperature (TN) of the film deposited at 360 °C at thicknesses ≥10 nm are also presented. In these two films the resistance in the thickness region 2≤d≤7.5 nm can be very well described by R∝[(d/dc)−1 ]−t with dc equal to 1.64±0.20 and 1.03±0.20 nm, respectively, and t=1.34±0.11. The Néel temperatures show a turning point around 14 nm in agreement with the known thickness dependence of the stress. dTN/dSt has been found to be ∼100 K/kbar where St is the internal tensile stress in the film.
No takes yet. Share an insight, caveat, or question.
Lourens et al. (1988) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: