In this study, alumina-forming austenitic steels with different compositions were designed and subjected to oxidation in air at 550–650°C for 100–300 h. Results show that after oxidation at 550°C, all samples developed a uniform blue oxide scale on surface. When temperature increased to 600°C, alloys with Al ≤ 3.0 wt.% exhibited varying degrees of severe oxidation. In contrast, the alloy containing 3.5 wt.% Al showed superior oxidation resistance, forming only a ∼100 nm-thick protective scale. This scale exhibits a three-layered structure, consisting of an inner Al 2 O 3 layer, an intermediate Cr 2 O 3 layer, and an outer Fe–Cr–Mn complex oxide layer. Notably, the intermediate Cr 2 O 3 layer forms coherent interfaces with both the inner and outer oxide layers. Compared with 2.5 wt.% Al alloy, 3.5 wt.% Al alloy exhibits a smoother and more continuous oxide scale, a significantly reduced thickness of the outer Fe–Cr–Mn oxide, and an approximately twofold increase in thickness of the inner Al 2 O 3 layer. After oxidation at 650°C, no severe oxidation was observed in alloys with Al contents above 1.5 wt.%, which is likely due to the decreasing critical Al concentration required for the formation of a continuous Al 2 O 3 scale at elevated temperatures.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: