This is the authors' abstract. We don't add key points for this paper.
Theoretically, the two-phase laminated configurations should have even much higher magnetoelectric (ME) effects—however, prior experimental studies have failed to find such an enhancement. Here, the authors report the unleashing of the potential of the (2-1) connectivity configuration: a piezofiber (one-dimension connectivity) layer laminated between two high-permeability magnetostrictive FeBSiC alloy ones (two-dimension connectivity) has near-ideal ME coupling. Very high ME effects of up to 22V∕cmOe (4×10−7s∕m) at 1Hz—an order of magnitude higher than the giant ones—have been found.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Dong et al. (2006) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: