Answers are grounded in this paper and cite their sources.
Submicron channel-length pentacene thin-film transistors (TFTs) were fabricated by electron beam lithography and a lift-off process. It was found that pentacene TFTs operated in the submicron channel length, but an enhancement of the off-stage leakage current and a large hysteresis were observed. By further investigation, we found that the large hysteresis observed in the submicron channel length was due to the moisture in the air. We also found a non-moisture-related degradation, in addition to a moisture-related one, by a time-dependent degradation measurement. It is of great importance both to avoid the moisture invasion and to reduce charging sites in the channel for reliable pentacene TFTs.
No takes yet. Share an insight, caveat, or question.
Kita et al. (2003) studied this question.