Pb(Mg 1/3 Nb 2/3 )O 3 –PbTiO 3 (PMN–PT) (70/30) thin films were deposited by pulsed laser deposition using two growth strategies: adsorption controlled deposition from lead‐rich targets (∼25–30 mass%) and lower‐temperature deposition ( T d ≤600°C) from targets containing a small amount of excess lead oxide (≤3 mass %). The substrates used were (001) SrRuO 3 /LaAlO 3 . Typical remanent polarization values ranged between 12 and 14 μC/cm 2 for these films. The longitudinal piezoelectric coefficient ( d 33,f ) was measured using in situ four‐circle X‐ray diffraction, and the transverse coefficient ( d 31,f or e 31,f ) was measured using the wafer flexure method. d 33,f and e 31,f coefficients of ∼300–350 pm/V and ∼−11 C/m 2 were calculated, respectively. In general, the piezoelectric coefficients and aging rates were strongly asymmetric, suggesting the presence of a polarization bias. The large, extremely stable piezoelectric response that results from poling parallel to the preferred polarization direction is attractive for miniaturized sensors and actuators.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Maria et al. (2005) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: