A modified ternary microemulsion polymerization was successfully used to prepare nanosized polystyrene (PS) microlatexes with high PS/surfactant weight ratios of up to 14:1. Cationic surfactants used were alkyltrimethylammonium bromides, C n TAB, where n is either 12, 14, or 16. A water-soluble initiator was used for the polymerization at room temperature, with moderate stirring. The latexes obtained are bluish-opaque and have been stable now for about 8 months. The process produced rather uniform ( D w / D n ≅ 1.10) latex particles of about 40 nm having high molar masses of PS ranging from 1.0 to 2.2 × 10 6 g/mol. This was obtained by first generating monomer-starved latex particles in a ternary microemulsion containing only 0.5−1.0 wt % styrene and 1.0 wt % cationic surfactant. The subsequent supply of styrene monomer to the polymerized microemulsion was delivered either through dropwise addition or via hollow-fiber feeding of monomer. The latter method was employed for the first time.
No takes yet. Share an insight, caveat, or question.
Xu et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: