Answers are grounded in this paper and cite their sources.
Bulk In2O3–Sc2O3 alloys were synthesized in a cubic phase (space group Ia3) with Sc2O3 content varying between 0 and 30 wt %. The lattice parameters of these alloys showed a linear dependence on the composition. Films were deposited on glass substrates at a temperature of 250 °C in an oxygen pressure of 10 mTorr using a pulsed laser deposition technique. Films with Sc2O3 composition varying between 0 and 10 weight percent show resistivities varying between 1.85×10−3 and 2.18×10−1 Ω cm, while their optical transparencies were more than 80% for wavelengths between 400 and 900 nm.