The crystallization of amorphous Sm x Fe 80−x B 20 melt spun ribbons is studied over an extended range of composition (0 < x < 8). Differential scanning calorimetry scans reveal different endo- and exothermic effects depending upon the composition. X-ray diffraction and Mössbauer studies for samples annealed at temperatures close to the onset of the first exothermic effect prove that, during the primary crystallization of the amorphous ribbons, both α-Fe and Fe 3 B phases appear—with Sm ions randomly accommodating the Fe sites in the tetragonal Fe 3 B lattice—while the subsequent exothermic reactions correspond to the decomposition of the metastable Fe 3 B phase into α-Fe and Fe 2 B and to the formation of the ternary Sm 1.1 Fe 4 B 4 phase. Fully crystallized ribbons with Sm contents lower than about 7 at.% show the co-existence between α-Fe and Fe 2 B soft magnetic phases and the Sm 2 Fe 14 B magnetic one. The enhancement of magnetic properties with increasing relative proportion of magnetic phase is discussed and correlated with exchange coupling and spin wave stiffness data obtained from the magnetic measurements.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Crisan et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: