Sm(Co0.70Fe0.21Cu0.06Zr0.03)7.6 sintered magnets with various Hci have been prepared by the conventional powder metallurgy method. Five magnets with Hci ranging from 15 to 40 kOe (at 25 °C) were selected to examine the impact of Hci on the irreversible loss and reversible temperature coefficient of induction (α). Magnets with higher Hci and Hk were found to exhibit lower irreversible losses when heated to 450 °C. Unlike the irreversible loss, α was found to be nearly independent of the Hci or Hk. These trends suggest that the irreversible loss is microstructure related and can be manipulated by process control, while α is more composition related and is dependent upon the overall chemical composition of the magnet. Br of 8.3 kG, Hc of 2.7 kOe, Hci of 3.5 kOe and BHmax of 6.7 MGOe at 450 °C were obtained on a Sm(Co0.70Fe0.21Cu0.06Zr0.03)7.6 magnet with a Hci of approximately 40 kOe at room temperature. Additional efforts are required to produce magnets which can be utilized at 450 °C.
No takes yet. Share an insight, caveat, or question.
C. O. Bounds (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: