Answers are grounded in this paper and cite their sources.
Demonstration of a 2.5-kV diamond diode is provided by electrical measurements using a circular gold Schottky contact, with an area >1 mm/sup 2/, on large area freestanding single-crystal diamond consisting of a thin high purity layer (1/spl times/0/sup 19/ [B]/cm/sup 3/) substrate with an ohmic back contact. The diode structures were fabricated using a microwave-assisted chemical vapor deposition process. The forward properties of the diode show a space charge limited current, with a forward-voltage drop of 2 V and a hole mobility of 4100/spl plusmn/400 cm/sup 2//Vs at room temperature. For temperatures between 300 K<T<380 K the mobility show T/sup -3/2/ dependence. This is consistent with acoustic phonon scattering, emphasizing the high purity quality of the top layer in which carrier transport is phonon rather than defect limited.
No takes yet. Share an insight, caveat, or question.
Twitchen et al. (2004) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: