c-axis-oriented ZnO films were prepared in O2 atmosphere by chemical vapor deposition using zinc acetylacetonate for source material. A minimum value of resistivity, 2.44 Ω cm, was obtained at a film formation temperature of 550 °C. The resistivity of the films was measured at low temperatures (87–297 K). For temperatures between 200 and 297 K band conduction included boundary scattering due to both thermionic emission and thermal-field emission at the grain-boundary barriers in the films, and the activation energy obtained ranged from 1.45 to 6.32×10−2 eV. For temperatures lower than about 200 K, the conductivity deviated from linear Arrhenius plots suggesting variable range-hopping conduction. Discussions based on assumed electron mobility and concentration lead to variable range-hopping conduction by localization of electrons in impurity levels in the intermediate concentration region. Mott’s parameters in the variable range-hopping conduction were estimated for the films.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Natsume et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: