Answers are grounded in this paper and cite their sources.
In vitro study demonstrates superior fracture resistance in CAD-CAM ceramic crowns cemented with adhesive resin cements, indicating improved durability over glass ionomer alternatives.
Background/Objectives: This in vitro study evaluated the fracture resistance of computer-aided design and computer-aided manufacturing (CAD-CAM) resin-matrix ceramic crowns cemented with three adhesive resin cements and three novel resin-modified glass ionomer cements. Methods: Ninety crowns representing a maxillary left central incisor were milled from a resin-based nanoceramic hybrid material (Cerasmart, GC) using a chairside CAD-CAM system (Primescan). The typodont preparation included 1.5-mm incisal reduction, 1.5-mm axial reduction, and a 1.0-mm chamfer finish line. Crowns were cemented onto 3D-printed dies of the preparation and assigned to six groups (n = 15 per group) according to cement type: Multilink Automix (ReMu), Panavia V5 (RePa), RelyX Unicem 2 (ReUn), RelyX Luting Plus (GiLu), GC FujiCem Evolve (GiEv), and Meron Plus QM (GiMe). The cemented restorations were subjected to artificial aging with 10,000 thermocycles at 5 to 55 °C with a dwell time of 30 s. Specimens were loaded in compression to fracture. Scanning electron microscopy (SEM) was used to evaluate fracture patterns. Fracture load was analyzed using one-way ANOVA and post hoc Tukey honestly significant difference (HSD) test (p = 0.001). Results: Fracture resistance differed significantly among cement types. Crowns cemented with adhesive resin cements exhibited higher fracture resistance than those cemented with resin-modified glass ionomer cements. The highest fracture resistance was observed for ReUn, followed by RePa and ReMu, whereas GiEv and GiLu showed the lowest values. Conclusions: CAD-CAM hybrid crowns fabricated from a resin composite–ceramic material demonstrated higher fracture resistance when cemented with adhesive resin cements than with the novel resin-modified glass ionomer cements tested. Among the six cements, ReUn produced the highest fracture resistance, whereas GiEv produced the lowest.
No takes yet. Share an insight, caveat, or question.
Jurado et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: