The effect of operating conditions on product yields and compositions has been studied in the catalytic cracking of polyolefins (high- and low-density polyethylene and polypropylene) in a conical spouted bed reactor. The catalyst has been prepared by agglomerating an HZSM-5 zeolite (SiO 2 /Al 2 O 3 = 30) with bentonite and alumina. The study has been carried out in continuous mode, in the 450–570 °C range, with polyolefin flow rates between 1 and 2 g min –1 and feeding up to 1 kg of polyolefin into a 30 g catalyst bed. The result is an excellent performance of the reactor–catalyst pairing for continuous catalytic pyrolysis, given that the yields obtained in the pyrolysis of high-density polyethylene at 500 °C without defluidization problems and very low catalyst deactivation are as follows: 60 wt % C 2 –C 4 olefins, 15 wt % nonaromatic C 5 –C 11 hydrocarbons, 10 wt % single-ring aromatics, and 14 wt % C 4- alkanes. Only small differences are observed in the pyrolysis of the different polyolefins.
No takes yet. Share an insight, caveat, or question.
Elordi et al. (2011) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: