Answers are grounded in this paper and cite their sources.
The interface trap density of states Dit of ultrathin SiO2 film has been investigated as a function of process variables. The process parameters used were oxidation temperature (1000–1200 °C), oxide thickness (4–10 nm), and annealing condition, including ambient (deuterium, argon, and in vacuum), temperature (500 and 900 °C), and time (10–120 s). Analysis of as-grown SiO2 films showed that the Dit decreases with increasing oxidation temperature and/or oxide thickness. With annealing in argon or in vacuum at 900 °C, the Dit decreases exponentially at the initial stage, then starts to increase linearly with increasing time. Similar behavior was observed for 900 °C deuterium annealing. Deuterium annealing at 500 °C was more effective in the reduction of the Dit, whereas argon annealing at the same temperature did not affect the density at all. A possible model for annealing kinetics is proposed to explain the experimental results.
No takes yet. Share an insight, caveat, or question.
Fukuda et al. (1992) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: