Precipitation-strengthened Cu alloys undergo channelized cyclic deformation, but its microstructural nature and orientation dependence remain unclear. In this study, a near-peak-aged Cu–3.15 mass% Ti alloy is subjected to low-cycle fatigue (ε p = 0.20%–1.00%) and interrupted at the stress-amplitude plateau. Correlative electron microscopy identifies the localizations as precipitate-free bands (PFBs), containing slip channels depleted of intact β′ precipitates without systematic band-scale Ti redistribution. High-resolution electron backscatter diffraction reveals that PFBs are zones of intense plastic localization, exhibiting high geometrically necessary dislocation densities (10 15 –10 16 m −2 ), continuous lattice rotations, and residual stress variations (∼10 2 MPa). Grain-scale probability maps reveal an amplitude-dependent orientation tendency: low Taylor-factor orientations are favored at ε p = 0.20%, whereas the product of directional Young’s modulus and maximum Schmid factor correlates more strongly at ε p = 0.50%. Orientation–based separation weakens near ε p ≈ 0.35%. Grain-level and population–averaged PFB coverage metrics describe localization intensity more robustly than highly scattered PFB widths. The study findings provide orientation- and coverage-based descriptors for assessing fatigue localization in precipitation–strengthened Cu alloys.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: