Answers are grounded in this paper and cite their sources.
The exchange bias and thermal properties of Pt1−xMnx–Cr∕NiFe films were investigated. Adding Cr into Pt1−xMnx film by inserting thin Cr layers was found to decrease the exchange bias considerably for x>0.5 but lead to a great enhancement of the pinning field along with unvarying coercivity and better thermal stability for x⩽0.5. An optimum pinning field of ∼180 Oe was obtained for Pt0.55Mn0.45–Cr(4%) pinning 150 Å NiFe—almost twice that of pure Pt0.55Mn0.45, and even larger than that of Pt0.5Mn0.5, by 20%. Although possessing a smaller grain size, Pt0.55Mn0.45–Cr(4%) has a higher blocking temperature than either pure Pt0.55Mn0.45 or Pt0.5Mn0.5. Structure characterization revealed that adding Cr promoted the ordering process of Pt1−xMnx (x⩽0.5) greatly, and a perfect ordering phase of Pt(MnCr) was formed. The present results suggest that PtMn–Cr has favorable properties as a pinning layer.
No takes yet. Share an insight, caveat, or question.
Dai et al. (2004) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: