This is the authors' abstract. We don't add key points for this paper.
Secondary ion mass spectroscopy (SIMS) has been used to measure the diffusion of deuterium in hydrogenated amorphous silicon. For a film deposited in a dc glow discharge in SiH4 at a substrate temperature of 315 °C, the diffusion data fits D (T) =1.17×10−2 exp(−1.53 eV/kT) cm2/s. This result implies that degradation of these films due to hydrogen out-diffusion at 100 °C will not be significant until after more than 104 years.