Starting from carefully homogenized Nd10Fe90-yMoy (y=12, 10, 7) alloys and by appropriate mechanical milling, the as-milled microstructure consisting of a nanoscale mixture of severely distorted 1:12 phase and substitutional α-Fe-based solid solution was obtained. This kind of as-milled microstructure was thought to have a critical effect on the formation of iron-free nanocrystalline 1:12 phase during subsequent annealing. Upon nitrogenation, the sample of Nd10Fe78Mo12Nx exhibited a record-high coercivity of 13.1 kOe at 293 K. Measurements of initial magnetization curve and a family of demagnetization curves engendered under different maximum applied fields Hm were carried out, and the results revealed the domain-wall pinning at grain boundaries as the coercivity mechanism. A low Mo-content sample of Nd10Fe83Mo7Nx with Hci∼5.8 kOe, Br∼6.8 kG, and (BH)max∼7.0 MG Oe was made by optimizing the preparation conditions.
No takes yet. Share an insight, caveat, or question.
Zhang et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: