Answers are grounded in this paper and cite their sources.
The solubility of As in Si as an active, noncomplexed dopant is determined by completely activating with laser annealing a metastable As concentration of about 1×1021/cm−3, and subjecting it to thermal-equilibrium annealing. The solubility is 9.3×1019 cm−3 at 700 °C and 3.2×1020 cm−3 at 1000 °C. MeV ion channeling measurements show that when As deactivation from the metastable concentration takes place at 900 °C, the As atoms stay almost completely substitutional. The deactivation process has a thermal activation energy of 2.0 eV at 350–410 °C.
No takes yet. Share an insight, caveat, or question.
Lietoila et al. (1980) studied this question.