For polycrystalline films of MnAs the complex index of refraction, N=n—ink, and the off-diagonal component of the complex dielectric tensor, Q=Q0 exp (-iq) were determined as functions of wave-length from 0.45 μm to 0.95 μm. The complex index of refraction increases from N=1.84-i1.75 at 0.45 μm to 2.13-i3.33 at 0.95 μm. Q0 and q increase from 0.008 and 29° at 0.45 μm to a maximum of 0.0194 and 55° at 0.9 μm, respectively. The dispersion of the Kerr rotation shows a change in sign at 0.72 μm. A maximum Kerr rotation of +0.058° is found at 0.9 μm and a maximum Kerr ellipticity of −0.15° at 0.72 μm. From these data a Faraday effect | 2F | = π | NQ|/λ0 of 156 000°/cm and an absorption coefficient α=4πnk/λ0 of 4.5×105/cm were calculated at 0.8 μm. The figure of merit is f=|2F|/α=0.34°. Also calculated were the complex dielectric constant ε and the reflectivity R. A description of the film preparation technique in high vacuum (10−7 Torr) is given. The films were analysed by x-ray diffraction techniques and were found to be stoichiometric MnAs.
No takes yet. Share an insight, caveat, or question.
Stoffel et al. (1970) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: