(Ta,W) and (Ta,W):C films with ~5 at.% C were deposited by non-reactive magnetron sputtering. They crystallised in a bcc structure with a columnar microstructure. The solid solubility of C in (Ta,W) alloys is very low, which suggests that the (Ta,W):C films are supersaturated with respect to carbon. This was confirmed by diffraction and atom probe tomography (APT) showing that carbon is in the as-deposited (Ta,W):C films homogeneously distributed in the structure without carbide formation or carbon segregation. Annealing at 900 °C for 2 h showed no significant column coarsening but an increased defect density at the column boundaries in the (Ta,W):C films. The films were still supersaturated with respect to carbon but APT showed a partial segregation of carbon presumably to defect-rich column boundaries after annealing. The (Ta,W) films exhibited a hardness of ~12–13 GPa. Alloying with carbon increased the hardness to ~17 GPa. The hardness increased to ~19 GPa for the annealed (Ta,W):C films. This annealing-induced hardness increase was explained by C segregation to the more defect-rich column boundaries, which restricts dislocation movements. (Ta,W):C coatings may be a potential alternative to ceramic coatings, worth exploring further by small scale mechanical testing to investigate if these materials are ductile.
No takes yet. Share an insight, caveat, or question.
Fritze et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: