Bi-2212/Ag phi 1-mm round untextured wires have been produced with critical current densities of 1200 A/cm/sup 2/ at 77 K, 0 T and up to about 2.0*10/sup 4/ A/cm/sup 2/ at 4.2 K in magnetic fields beyond 20 T. In order to achieve this, a two-step annealing procedure is necessary with a partial melting of the wire core, the melt having a composition near Bi/sub 2/(Sr,Ca)/sub 2/Cu/sub 1/O/sub 6+x/. On cooling, the Bi/sub 2/(Sr,Ca)/sub 2/Cu/sub 1/O/sub 6+x/ phase appears at 880 degrees C, as revealed by in situ XRD (X-ray diffraction) measurements. Long-term annealing at 840 degrees C leads to the transformation of this phase into the Bi/sub 2/Sr/sub 2/Ca/sub 1/ Cu/sub 2/O/sub 8+x/ phase. The alkaline earth cuprate (Sr,Ca) /sub 14/Cu/sub 24/O/sub approximately=40/ and CuO occur as major extraneous phases. Helically shaped samples yield a lower j/sub c/ between 3*10/sup 3/ and maximum 1.0*10/sup 4/ A/cm/sup 2/ at 4.2 K, 10 T. Cracks due to thermal expansion mismatch with the sample holder and remaining inhomogeneities along the wire are responsible for these lower values. From I-V curves measured at 4.2 K, n-values were determined to be 20 to 25 in the interesting very-high-field region beyond 20 T. Bi-2223/Ag highly textured thin tapes yield an appreciably higher j/sub c/ of 2.6*10/sup 4/ A/cm/sup 2/ at 77 K, 0 T. Temperature-dependent measurements of j/sub c/ as a function of magnetic field B yielded onset of significant flux creep above 20 K, limiting the range of application in magnet technology to the temperature range up to 20 K unless an additional more effective pinning mechanism is introduced.
No takes yet. Share an insight, caveat, or question.
Tenbrink et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: