Alumina and Al 2 O 3 /ZrO 2 (1 to 10 vol%) composite powders were mixed and consolidated by a colloidal method, sintered to >98% theoretical density at 1550°C, and subsequently heat‐treated at temperatures up to 1700°C for grain‐size measurements. Within the temperature range studied, the ZrO 2 inclusions exhibited sufficient self‐diffusion to move with the Al 2 O 3 4‐grain junctions during grain growth. Growth of the ZrO 2 , inclusions occurred by coalescence. The inclusions exerted a dragging force at the 4‐grain junctions to limit grain growth. Abnormal grain growth occurred when the inclusion distribution was not sufficiently uniform to hinder the growth of all Al 2 O 3 grains. This condition was observed for compositions containing ≤2.5 vol% ZrO 2 , where the inclusions did not fill all 4‐grain junctions. Exaggerated grains consumed both neighboring grains and ZrO 2 , inclusions. Grain‐growth control (no abnormal grain growth) was achieved when a majority (or all) 4‐grain junctions contained a ZrO 2 inclusion, viz., for compositions containing ≥5 vol% ZrO 2 . For this condition, the grain size was inversely proportional to the volume fraction of the inclusions. Since the ZrO 2 inclusions mimic voids in all ways except that they do not disappear, it is hypothesized that abnormal grain growth in single‐phase materials is a result of a nonuniform distribution of voids during the last stage of sintering.
No takes yet. Share an insight, caveat, or question.
Lange et al. (1984) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: