Changes in bulk density, shrinkage, and weight are given for carbon and for dry‐pressed specimens of beryllia, magnesia, zirconia, thoria, molybdenum, and tungsten when fired for 2, 4, and 8 minutes under vacuum conditions, using 100 °C. increments, in the temperature range 1500° to 2300°C. Temperatures at which instability of surface‐to‐surface contact was observed for the twenty‐one possible binary systems of the foregoing substances are also described for identical conditions of testing.
No takes yet. Share an insight, caveat, or question.
P. D. Johnson (1950) studied this question.