In this paper, Ag-Zn alloy are dealloyed in 0.1M H2SO4 at a low temperature (2°C) to fabricate nanoporous silver and the dealloying kinetics has been systematically investigated. Comparison of the polarization curve of Ag-Zn alloy in 0.1M H2SO4 at room temperature and 2°C shows that lowering temperature can significantly reduce the diffusivity of silver atoms and result in forming more exiguous nanoporous silver. SEM observation demonstrates that pores have formed on initial of the dealloying process. The succeeding process just coarsenes pores by silver atoms diffusion and aggregation at the silver/electrolyte interface due to the structure is on a instability state in thermodynamics in the electrolyte. Pore size can grow from tens of nanometers to hundreds of nanometers with the extension of dealloying time in the electrolyte without else treatment. The coarsening exponent and surface diffusivity of silver atoms are estimated to be 4.19 and 1.2×10-16 m2/s. There also exists phase transition in the dealloying process. The forming mechanism of nanoporous silver at low temperature is discussed in the end.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Li et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: