A constant stress testing machine of small inertia and with continuous strain recording has been built. The loading was by air contained in metallic bellows whose wall stiffness was compensated by a `negative spring'. The initial strain rate was standardized at 1% per second. Polycrystalline copper and aluminium have been investigated between -196°C and 140°C. At low temperatures, the creep curves fitted = α log t + c 1 ; at higher temperatures they fitted = β t 1/3 + c 2 . These are called α and β creep respectively. In an intermediate temperature range the curves fitted = α log t + β t 1/3 + c 3 . The results have been confirmed for cadmium and commercially pure aluminium, and also for aluminium with only a few grains per specimen. In a series of increment tests the stress was altered by small amounts at various times during a creep curve; in the α range only, the curves after the increments were similar to segments of the parent curve. The effect of testing a specimen at increasing stresses and different temperatures was also investigated; in the α range only, an equation of state, that is F (σ, , d / dt, T ) = 0, was obeyed. A theory of α creep is developed: an exhaustion theory is applied to a metal whose strain hardening is defined by a reference curve. The rise of activation stress during a creep curve and the slope of the reference curve are deduced from the increment and creep tests; and the slope agrees numerically with the stress-strain curve at -196°C. From an equation of state, values of the mean activation energy at a strain rate of 10 -4 cm/cm/sec, and the frequency of thermal fluctuations are obtained.
No takes yet. Share an insight, caveat, or question.
Oliver H. Wyatt (1953) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: