This is the authors' abstract. We don't add key points for this paper.
Amorphous SiO 2 (a-SiO 2 ) films were deposited at 300°C by plasma-enhanced chemical vapor deposition using SiH 4 –O 2 mixtures. The [O 2 ]/[SiH 4 ] ratio was maintained at 1.5, in which oxide films having a stoichiometric composition could be obtained. The Si–O–Si stretching mode, stress, the density of Si dangling bonds and buffered HF (BHF) etch rate were investigated as a function of film thickness. It was found that the peak frequency of Si–O–Si stretching mode centered at around 1050 cm -1 increased from 1050 to 1075 cm -1 with increasing film thickness from 0.1 to 1.1 µm. By comparison with calculations based on the effect of multiple reflections in film/substrate system, it was found that the shift of the Si–O–Si stretching mode to high frequencies was due not only to the effect of multiple reflections, but also to the physical effect of thermal heating and/or ion bombardment during film growth, which would contribute to rearrangement of the Si–O–Si bonding network. The experimental results for the stress behavior, the density of Si dangling bonds and BHF etch rate confirmed this finding.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
He et al. (2001) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: