The rate of sorption of thorium powder for oxygen and hydrogen is measured at pressures between 10 -7 and 10 -3 mm mercury as a function of temperature of the thorium and of the period of exposure to gas. The sorbed quantities of gas are determined from the variation of rate of sorption with time. It is found that oxygen is sorbed irreversibly, forming a stable oxide with a dissociation pressure which is immeasurably low. The activation energy of this chemisorption is ascertained from the increase of rate of sorption with temperature of the thorium and is found to be about 0.75 kcal/mol. Hydrogen is sorbed reversibly by a process of solution. The correlations between sorbed quantity of hydrogen, hydrogen pressure and temperature of the thorium are those to be expected for an equilibrium of solution. During dissolution of hydrogen heat is evolved and a value of about 13 kcal is found for this heat of solution. There are indications that at very low pressures most of the hydrogen in a tube containing thorium powder is in the atomic state. The rate of sorption for hydrogen has a maximum value between 700 and 750°K. The significance of these results for the application of getter materials in electronic valves is discussed briefly.
No takes yet. Share an insight, caveat, or question.
Siegfried Wagener (1953) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: