Answers are grounded in this paper and cite their sources.
The linear thermal expansions of the following 36 materials were measured: African chrome sand; Cuban, Grecian, Friable African, Rhodesian Imperial, Indian and Turkish chrome ores; Austrian, Californian, and electrically fused magnesites; a periclase brick; a spinel brick; two types of fire-clay bricks and two of fire clays; Kentucky, Tennessee, and English ball clays; Georgia kaolin and and English china clay; an 80 percent alumina brick; artificial corundum, dia- spore, bauxite; five mullites, each of which was prepared from different raw materials; two zircon bricks and afurnaced zirconium silicate; silicon carbide, a silica brick, and an insulating brick.Data are also given on artificial graphite which had been preheated several times to 1,800° C. Measurements were made below 1,000° C. in both an oxidizing and a reducing atmosphere.Above, 1,000° C. the materials were tested in a reducing atmosphere only.When the refractoriness of the materials permitted they were tested up to 1,800° C. Petrographic analyses of the materials were made before and after the several heat treatments.
No takes yet. Share an insight, caveat, or question.
R.A. Heindl (1933) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: