Answers are grounded in this paper and cite their sources.
The high temperature properties of Poly(p-phenylene-2,6-benzobisoxazole) (PBO) fiber are examined and compared with those of the p-Aramid fiber. In particular, the temperature dependence of tensile strength of the PBO fiber is reported for the first time. The PBO fiber has 100°C higher decomposition temperature than the p-Aramid fiber, and the amount of toxic gases in combustion is much smaller than the p-Aramid fiber. Although the relative strength decreased proportionally in the range of room temperature to 500°C, the PBO fiber has 40% of the strength at room temperature even at a temperature of 500°C. After thermal treatment at 500°C for 60 s, the PBO fiber retained 90% of its original strength. The PBO fiber is expected to substitute for asbestos, which is still used as a heat resistant cushion material.
No takes yet. Share an insight, caveat, or question.
Kuroki et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: