Answers are grounded in this paper and cite their sources.
We report the growth of oriented PbZrxTi1-xO3 (PZT) films, formed in situ by pulsed laser deposition onto heated substrates. The films were deposited from a pressed pellet of PbO - ZrO2 - PbTiO3 of composition PbZr.54Ti.46O3 using a KrF excimer laser (248 nm, ∽2 J/cm2, 5 hz). Typically, 300 to 1500-nm-thick films were deposited onto a heated substrate of <100> MgO or <100> SrTiO3. The deposition temperature was varied from RT to 750°C in ambient oxygen pressures between 10-6 and 0.3 Torr. Films were analyzed form structure (XRD), composition and thickness (EBS), and surface morphology (SEM). For substrate temperatures up to at least 250°C, an amorphous film was deposited. Isochronal annealing of such a film produced crystallization only after heating for 1 h at 550°C. In contrast, crystalline films were deposited at temperatures as low as 350°C, although <100gt; oriented PZT required at least 550°C. Films deposited beyond 600°C, or in too low an oxygen pressure were Pb deficient.
No takes yet. Share an insight, caveat, or question.
Grabowski et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: