Answers are grounded in this paper and cite their sources.
A post-weld annealing strategy was developed to control the high-cycle fatigue performance of dissimilar TC11/TC17 titanium alloy linear friction welded joints. By systematically varying the stress relief annealing temperature (590, 605, 630, and 650 °C), the microstructural evolution, residual stress, and mechanical properties were investigated. The results demonstrate that increasing the annealing temperature promotes the decomposition of metastable β phase and the precipitation of fine secondary α, which raises the α phase area fraction in the fracture zone; this effect saturates above 630 °C. Concurrently, the longitudinal tensile residual stress, which reaches 400 MPa in the as-welded state, is substantially relaxed and is essentially eliminated at 630 °C. These synergistic changes enable a monotonic increase in the fatigue limit from 453.3 MPa to 512.5 MPa as the temperature rises to 630 °C, after which the property stabilizes. Fracture toughness exhibits divergent trends among the weld zones: the KIC of the weld nugget zone and the TC17-side thermo-mechanically affected zone increases with annealing temperature, while that of the TC11-side zone decreases due to the globularization of lamellar α; all three zones stabilize at approximately 33 MPa m 1/2 and 40 MPa m 1/2 , respectively. Integrating the microstructural evolution, residual stress relief, and mechanical property improvements, the optimal stress relief annealing strategy is to apply a temperature of at least 630 °C, which ensures superior fatigue resistance and microstructural stability for TC11/TC17 linear friction welded joints.
No takes yet. Share an insight, caveat, or question.
Shen et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: