Answers are grounded in this paper and cite their sources.
Effects of K nonstoichiometry and Li addition on piezoelectric and dielectric properties of (Bi0.5K0.5+xLiy)TiO3 ceramics were studied in the range of x=−8–1 and y=0–5 mol % from the stoichiometric K0.5. A tetragonal perovskite structure was maintained at all compositions despite the formation of secondary phases with K deficiency. Piezoelectric coefficient (d33) was improved from 13 pC/N at x=0 mol % to 32 pC/N at x=−5 mol % due to K vacancies facilitating domain walls movement. It was further enhanced showing a peak value of 103 pC/N at x=−5 and y=3 mol % due to the microstructure improved with the tetragonality optimized by Li addition.