Ferroelectric symmetric superlattices consisting of alternating layers of PbTiO3 and PbZr0.2Ti0.8O3, were grown by pulsed laser deposition on SrTiO3 and SrRuO3-coated SrTiO3 substrates. The superlattices, with wavelengths Λ ranging from 20 Å to 200 Å, were analyzed using x-ray diffraction (θ−2θ diffraction scans, rocking curves, and reciprocal space mapping), high resolution transmission electron microscopy, and piezoforce scanning microscopy. For large-period superlattices, the strain is relieved by the formation of an a/c polydomain structure which propagates through the whole film. We investigate the influence of the wavelength on the a-domain volume fraction, the lattice parameters, the in-plane strain εxx, and the mosaicity of the samples. We show that with decreasing the wavelength, a reduction of the a-domain volume fraction is observed as well as a reduced tensile in-plane strain and a lower mosaicity. A concomitant improvement of the local ferroelectric response is detected. Below a critical wavelength of about 30 Å and a critical sample thickness of 500 Å, the formation of 90° a/c domains is inhibited and the superlattices are completely c oriented. Thus the reduced wavelength induces compressive strain which dominates over the tensile clamping due to the thermal expansion mismatch between the substrate and the superlattice. This compressive strain favors a c-oriented structure in the PbTiO3/PbZr0.2Ti0.8O3 superlattices.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Hubault et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: