Answers are grounded in this paper and cite their sources.
Ten compositions were prepared in the systems As:Se:Te and As:S:Te. Nine of these compositions were amorphous in structure. The resistivities and Seebeck coefficients of these materials were measured as functions of temperature. The resistivity varied exponentially with temperature, while the Seebeck coefficient varied linearly. At 298°K, the resistivity values for the amorphous samples ranged from 4.7×104−2.5×1013 ohm-cm, while the Seebeck coefficient values ranged from 830–1625 μv/°K (p type). At any temperature, the resistivity decreased with increase in tellurium content. For the amorphous materials, the thermal conductivity values ranged from 2.4–4.4 mw/cm-°K.
No takes yet. Share an insight, caveat, or question.
Uphoff et al. (1961) studied this question.