In this study coaxial composite all-aluminium wire (CAAW), made of electromagnetically cast Al-0,5Fe (core) and Al-1,7Fe (sleeve) alloys, was produced by cold drawing and subjected to annealing at 230 °C for 1h. Core alloy area fraction in CAAW was 0%, 10%, 30%, 50% and 100%, which corresponds to 0, 0,32, 0,55, 0,70 and 1 of the boundary between constituents as a fraction of the outer wire diameter, respectively. Rule of mixtures was implemented to calculate the CAAW’s expected levels of electrical conductivity, ultimate tensile strength and elongation to failure. Experimental data was compared to the IEC 62641-2023 standard for conductive aluminium wires. It was demonstrated that produced CAAWs mostly meet the requirements of the commercial standard. Rule of mixtures predictions have highest deviation from the experimental data in the 0,3-0,5 core alloy fraction range, meaning that these properties are boundary-driven. CAAWs exhibit the decrease in ductility and increase in ultimate tensile strength during annealing due to the presence of Al-1,7Fe alloy, which was as well reported in previous studies. For these properties’ changes the CAAWs could be considered thermally resistant. Visual representation of the experimental data combined with rule of mixtures predictions allow to prognose the CAAW with certain composition that will meet the targeted level of properties.
No takes yet. Share an insight, caveat, or question.
Medvedev et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: