This is the authors' abstract. We don't add key points for this paper.
The adiabatic elastic constants of a single crystal of indium antimonide have been measured by an ultrasonic pulse technique in which 10-Mc/sec acoustic waves were employed. The elastic constants extrapolated to 0^∘{}K are, in units of 10¹² dynes/cm², c₁₁=0.6918, c₁₂=0.3788, and c₄₄=0.3132. A Debye characteristic temperature, θ, of 205^∘{}±{}2^∘{}K at 0^∘{}K was calculated from these values of the elastic constants.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Slutsky et al. (1959) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: