In previous work the thermoluminescence of golden sapphire (Al2O3 containing Ni and Mg), which was γ irradiated under liquid nitrogen, was compared with glow curves of fused borax seeded with Ni and Mg. The emission intensity obeyed, reasonably well, the expression I=αN0k′ exp[−1/(dT/dt) ∫ t0tk′dT]. In the present paper it is shown that light-induced glow curves in γ-irradiated sapphire have the form of a second-order decay process, namely I = I0[b / (b+t)]m. Gamma-ray induced thermoluminescence in ruby shows dominant emission bands with maxima at about 150°K and 240°K. Light-induced thermoluminescence in γ-ray damaged ruby shows an afterglow long after the crystal has reached room temperature.