Answers are grounded in this paper and cite their sources.
Piezoelectric properties have been studied on ferroelectric ceramics comprising bismuth compounds with layer structure, PbBi 2 Nb 2 O 9 , PbBi 4 Ti 4 O 15 , SrBi 4 Ti 4 O 15 and Na 0.5 Bi 4.5 Ti 4 O 15 . These ceramics have the high mechanical quality factor Q (2000∼7200), low aging rate of frequency constant N t (30∼60 ppm/time decade), low temperature coefficients both of N t (-50 ppm/°C) and of coupling factor k t (70 ppm/°C), low Poisson's ratio σ(0.23∼0.27), and large anisotropy in coupling factor. A small value of k t in these ceramics probably relates to two-dimensional restriction on permissible rotation of the spontaneous polarization. The poling characteristics in the ceramics can be improved by some additives. Grain boundaries in these ceramics are of nearly rectangular shape, and an etch pattern of fine stripes appears always in parallel to the length of the boundary.
No takes yet. Share an insight, caveat, or question.
Ikegami et al. (1974) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: