Answers are grounded in this paper and cite their sources.
Plasma-free defect passivation is achieved on polycrystalline silicon thin-film transistors fabricated below 150°C by annealing and extracting H from SiNx:H interlayer dielectric. By annealing at 250°C without a plasma application, VT and μFE were improved from 11.5Vto3.5V and from 86cm2∕Vsto212cm2∕Vs, respectively. Improvement in performance is attributed to defect passivation by H diffusing out from SiNx:H. Dangling bonds and strained bonds can be acceptably passivated around 170°C, and 205°C, respectively. The activation energy for the diffusion of H into polycrystalline silicon was estimated to be 0.87eV.
No takes yet. Share an insight, caveat, or question.
Chung et al. (2006) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: