Answers are grounded in this paper and cite their sources.
Aqueous corrosion, atmospheric corrosion, and ionic liquid dissolution studies were performed on commercial alloys AZ31B, AM60, and AZ91D and compared with previously reported results for single-phase binary Mg–Al alloys containing similar Al concentrations (αMg-2 at% Al, αMg-5 at% Al, and Mg-8 at% Al). Polarization studies in 0.6 M NaCl were used to characterize the aqueous free corrosion behavior during 20-h free immersion. Accelerated corrosion testing was performed using a rotating-disk electrode which revealed the evolution of an Al-rich mud-cracking and platelet morphology. Atmospheric droplet testing showed rapid pH increases that depended on the Al concentration in the alloy. Time-dependent contact angle measurements showed that the degree of droplet wetting increased during free corrosion by ∼50° over 20 h in 0.6 M NaCl. Ionic liquid dissolution studies in 1:2 M choline chloride:urea deep eutectic solvent were performed in order to examine the current-voltage behavior of these alloys in the absence of water and hydrogen reduction. The results of these studies revealed the formation of nanowire corrosion morphologies within a honeycomb lattice structure which we attribute to selective dissolution of Mg via a two-dimensional step-flow process.
No takes yet. Share an insight, caveat, or question.
Aiello et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: